Since I have been for the most part stuck at home for the last three  or four days. Hospital stays are not fun not going back for a few years.

only 28 more 20 cell batteries to go
 I thought I would try nickel plating thanks to not2bme and the links he posted.

These will be for the posts on the BYD batteries. They are split on the back side of the tee. Still needs work have to remember to rinse off the parts (new copper refrigeration tees) after dipping inisopropyl alcohol. Either the alcohol  or the new 1/8 inch refrigeration tubing caused some of the plating to flake off.

later floyd
Oz18650 likes this post